Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kraton D1192 E - SBS - Kraton Polymers

Material Data Center offers the following functions for Kraton D1192 E:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kraton D datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
Kraton D1192 E is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass.
Технологические и физические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Показатель текучести расплава, ПТР 1 г/10 мин ISO 1133
Температура 200 °C -
Нагрузка 5 kg -
Механические свойстваЗначениеЕдиницаСтандарт
Данные ISO
предел прочности при растяжении 33 МПа ISO 37
Удлинение при разрыве 1000 % ISO 37
Данные ASTM
Твердость по Шору А 70 - ASTM D 2240
Other Standards[S]
Напряжение при 300%-ном растяжении 14.4 МПа ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
Прочие свойстваЗначениеЕдиницаСтандарт
насыпная плотность 400 кг/м³ -
Other Standards[S]
Плотность 940 кг/м³ ISO 2781
S: These properties are reported by the producer according standards that are different to our defaults.
Особые свойства и характеристики
Способы переработки
Нанесение покрытий
Особые показатели
Прозрачный
Специальные характеристики
Сополимер
Химическая стойкость
Стойкость к окислению
Доступность материала по регионам
Северная Америка, Европа, Страны Азии и Тихого океана, Ближний Восток и Африка
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com